Six defects for casting foundry part, read it, and problem resolved!
First, air holes (bubbles, boring holes, air pockets) Reasons: 1. The mould preheat temperature is too low, and the liquid metal is cooling too quickly
First, air holes (bubbles, boring holes, air pockets) Reasons: 1. The mould preheat temperature is too low, and the liquid metal is cooling too quickly